Lesson 5: Leave the plate in the silver nitrate for at least three minutes

December 1, 2012 · by glassplate | 1 Comment

Silver nitrate is very important, it can make or break an image very easily, despite knowing this fact, it is all too easy to try to speed up the waiting time. These two images were taken within a short time, light conditions were the same, timing was the same, temperature was the same, but I […]

Post navigation

Recent Posts

  • Bubbling Emulsion
  • Kurt Sorensen: Wet Plate Interview
  • Fractious Light and Fortuitous Scratches
  • Back in the Fray
  • Lesson 6: Collodion

Archives

  • April 2016
  • November 2014
  • September 2014
  • June 2013
  • January 2013
  • December 2012
  • November 2012

Categories

  • Lessons

Meta

  • Create account
  • Log in
  • Entries feed
  • Comments feed
  • WordPress.com
Blog at WordPress.com.
Privacy & Cookies: This site uses cookies. By continuing to use this website, you agree to their use.
To find out more, including how to control cookies, see here: Cookie Policy
  • Subscribe Subscribed
    • This Is Not Digital
    • Already have a WordPress.com account? Log in now.
    • This Is Not Digital
    • Subscribe Subscribed
    • Sign up
    • Log in
    • Report this content
    • View site in Reader
    • Manage subscriptions
    • Collapse this bar
 

Loading Comments...